Technology Zone

Bondtec

Bondtec covers the surface and bonding techniques that change what a textile can do. This zone covers plasma and chemical surface treatment, thermal, ultrasonic and adhesive bonding, lamination and the machinery behind them.

All articles in this zone

Bondtec — page 1 of 1

Back to the zone

What this zone covers

Bondtec: how it works, key numbers and troubleshooting

Fundamentals

Surface energy decides adhesion

Nothing sticks to a surface that will not wet. Polyolefins, polyester and most technical fibres have a surface energy too low for an adhesive to spread, so the first step is raising it: corona discharge for film and web, atmospheric plasma for three-dimensional and delicate substrates, low pressure plasma for the most demanding work, or a chemical primer. The treatment decays within hours to days, so bonding follows treatment closely or it does not work at all.

Thermal bonding and welding

Where the material is thermoplastic, the material itself becomes the adhesive. Hot air and hot wedge welding melt the surfaces and press them together, and they carry most tarpaulin and membrane seaming. Ultrasonic welding puts high frequency vibration into a small area, which is fast, clean and needs no consumable, and it is why hygiene and medical converting lines are full of ultrasonic horns. High frequency welding suits polar polymers such as PVC and polyurethane.

Adhesive bonding

Adhesives cover everything welding cannot: different polymers, non-melting fibres, and joints that need flexibility. Hot melt adhesives are applied as film, web, powder or spray and reactivate with heat, and they are what most laminating lines use. Reactive polyurethane hot melts crosslink after application with moisture and give far better heat and wash resistance. Solvent and water-based systems still hold their place where a very thin, uniform layer is needed.

Lamination

Laminating bonds two or more layers into one composite fabric: a face, a membrane and a backing, for instance. Flame lamination melts a foam layer and is fast and cheap but restricted by emissions rules. Adhesive lamination with a dot or web pattern preserves breathability and handle, and the pattern coverage is the setting that trades bond strength against drape. The bond must survive the wash cycles the product will see.

Testing the joint, not the material

A bonded assembly fails at the interface long before either material fails. That means peel strength, shear strength and, above all, the same tests after heat ageing, humidity and washing. A joint that peels at 60 newtons fresh and 15 after ten washes is a joint that will come back. Where the joint is safety relevant, destructive testing of production samples belongs in the routine, not in the qualification file only.

Key parameters

Parameter Typical range Rule of thumb
Surface energy targetAbove 38 dyne/cm, 44 and up for demanding bondsMeasure with test inks before bonding; do not assume the treater worked
Corona treatment decayEffective for hours to a few daysTreat in line with bonding wherever possible
Ultrasonic frequency20, 30 or 35 kHzLower frequency for thicker material, higher for fine and delicate webs
Hot melt coat weight5 to 30 g/m2 for laminatingMore adhesive means a stiffer, less breathable laminate, not a better one
Dot coverage10 to 30 % of the areaCoverage trades bond strength against handle and breathability
Welding temperature windowWithin 10 to 20 degrees of the optimumEstablish a window by trial and peel test, then control the middle of it
Peel strength20 to 100 N/50 mm depending on constructionSpecify after wash and heat ageing, not fresh
Reactive hot melt cure24 to 72 hours at ambient humidityDo not test or ship before the crosslink has finished

Troubleshooting

Symptom Likely causes What to do
Laminate delaminates after washingAdhesive not rated for the wash temperature, insufficient coat weight, or a reactive system tested before cureMove to a reactive polyurethane hot melt, verify the cure time, and test after the full wash cycle count
Bond fails immediately at the interfaceSurface energy too low, treatment decayed, or a silicone finish on the substrateMeasure with test inks, treat in line, and remove or ban silicone from the process
Ultrasonic weld cuts through the webAmplitude or pressure too high, wrong anvil pattern, or dwell too longLower the amplitude, change the anvil pattern to spread the energy, and reduce dwell
Welded seam is strong but stiff and brittleOverheating, too wide a weld, or a material welded outside its windowEstablish the temperature window with peel tests and run in the middle, and narrow the weld where the design allows
Laminate is stiff and no longer breathesCoat weight too high or dot coverage too greatReduce coverage, use a finer dot pattern, and re-test breathability against the specification
Adhesive strikes through to the faceCoat weight too high, temperature too high at the nip, or an open face fabricLower the coat weight and nip temperature, and consider a web adhesive rather than a coating
Bond strength varies across the widthUneven treatment, uneven adhesive application, or nip pressure not parallelProfile the treatment and the nip across the width, and check roller wear

Go deeper: news and case studies · frequently asked questions

Equipment Guide

Bondtec in the Equipment Guide

All manufacturers in this zone

8 equipment types

Recommended manufacturers

Do you manufacture bondtec equipment? A basic listing in the Equipment Guide is free.

Ask the Expert

Ask a bondtec expert — free

View all experts

Engineers and product specialists who answer technical questions from readers. The answer comes back to you by e-mail; when we publish it, other readers benefit too.

No field expert for this zone yet — your question still reaches our editors.

Subscribe to our E-newsletters

"*" indicates required fields

Name
Weekly E-Update (delivered every Tuesday)
E-Product Newsletters
Market Insight Newsletters

Questions and answers

Frequently asked about bondtec

Weld or glue?

Weld where both materials are thermoplastic and compatible, because there is no consumable, no cure time and no third chemistry to fail. Glue where they are not: different polymers, non-melting fibres, or a joint that has to stay flexible. Welding also gives a cleaner product for medical and hygiene use, which is why ultrasonic converting dominates those lines.

Why does surface treatment stop working?

Because it is not permanent. Corona and plasma raise surface energy by oxidising the top molecular layers, and those layers reorganise over hours to days, faster when it is warm. Treat as close to bonding as the line allows, verify with test inks rather than assuming, and remember that a treated roll stored for a week is effectively untreated.

Which adhesive for a washable laminate?

A reactive polyurethane hot melt, in nearly all cases. It applies like a hot melt and then crosslinks with ambient moisture, which gives it the heat and wash resistance that a plain hot melt lacks. The catch is the cure time: 24 to 72 hours before it reaches full strength, so do not test or ship on the same day and expect the final numbers.

How much adhesive should a laminate have?

Less than instinct suggests. More adhesive gives a stiffer, less breathable laminate and does not reliably give a stronger bond, because the failure is usually at the interface rather than in the adhesive layer. Dot patterns at 10 to 30 percent coverage give the balance most products want, and a finer dot at the same coverage gives a softer result.

Can ultrasonic welding handle any fabric?

Any thermoplastic one, and the proportion matters: a blend with too much natural fibre will not weld because there is not enough polymer to fuse. Fabric weight, anvil pattern, amplitude and dwell all interact, and the usual failure is too much energy cutting through the web rather than too little. It is fast, clean and consumable-free where the material allows it.

How should I specify bond strength?

As peel strength in newtons per fifty millimetres, tested after the ageing the product will see: wash cycles, heat, humidity, or all three. A fresh peel value is easy to hit and tells you nothing about the third summer. For safety relevant joints, put destructive testing of production samples into the routine rather than relying on the original qualification.

Is flame lamination still used?

Less every year. It is fast and cheap and needs no adhesive, but it burns a layer of foam to make the bond, which brings emissions that are increasingly hard to permit, and it limits the materials to those that will flame laminate at all. Adhesive lamination with a dot pattern has taken over most of the work, with better control over handle and breathability.

What is the difference between this Technology Zone and the Equipment Guide?

The zone is the editorial side: news, case studies, videos, newsletter editions and field experts. The Equipment Guide is the directory side: equipment types and the manufacturers that build them. This page links to its Equipment Guide category and back.

How do I find a manufacturer of bondtec equipment?

Open the Equipment Guide category for this zone, pick an equipment type and open a manufacturer profile. Partner profiles carry direct contact details; other listings link to the company website.

Can I ask a technical question before I buy?

Yes. Ask the Expert puts your question to a field expert in this zone. The answer comes back to you by e-mail; when we publish it, other readers benefit too.

Your company in this zone?

Do you manufacture technical textiles and want your company in a market? A basic listing is free.

List your company